Site gates do not fail at the leaf. The welded mesh panel stays square for years while the hinge fixing, the latch and the temporary fencing drop bolt accumulate the clearance that makes a gate scrape. The sag sits at the bolt-to-hole interface — a specification question long before it is a maintenance one.
One gate-hardware table is published on this site, on the farm gate hinge and latch product page, and it gives four columns worth arguing about: three gudgeon routes (through, screw-in, drive-in), one stud of ø20 × 70 mm, thread lengths of 300 mm or 350 mm on the through version against 150 mm or 200 mm on the other two, and washers and nuts as the fitting. Those are published figures, not a duty rating — the way to use them is to put them beside your own post section and get the match confirmed in writing.
Key Takeaways
- The farm gate hinge and latch page itemises three gudgeon types on one ø20 × 70 mm stud: 300 mm or 350 mm of thread through a post, 150 mm or 200 mm for the screw-in and drive-in routes, washers and nuts as the fitting. Published figures — confirm them against your own post section before ordering.
- A gate’s mass goes into the fixing, not the hinge leaf. Engaged thread length and the condition of the hole around it decide whether the leaf still swings level after a season of hand use.
- A latch and a drop bolt solve different failures. The latch keeps the leaf shut; the bolt holds it in line with the frame so it cannot rake.
- No load rating is published. That page carries one sentence about withstanding heavy loads and names two finishes — hot dip galvanising or dacromet — and the finish argument lives in this site’s guide to fence fittings corrosion.
- Six lines settle a gate order: gudgeon route, stud and engaged thread length, post size and wall, latch or bolt per leaf, finish, and spares as a count.
In this guide
Three Gudgeon Routes, Three Ways to Drop
A gudgeon is the plain term for the hinge boss a gate hangs on. The published page splits its hinge line three ways by how the stud gets into the post. Read it with one caveat: that table sits on a farm gate hinge page, so the first written question for a site gate is whether the same studs and thread bands are what your gate ships with.
The through gudgeon is published with 300 mm or 350 mm of thread and passes right through the post, finishing with washers and nuts on the far side. It is the only one of the three where clamping force is independent of what the post material will hold, and the only one you can re-tighten from outside once clearance starts to build. The screw-in and drive-in versions are published at 150 mm or 200 mm. Their holding power is whatever that short thread engages inside the post.
A fence post is a tube, and no page read for this article publishes a wall thickness for site gate posts. That is exactly why a short internal thread is a gamble: 150 mm engaged inside a hollow tube is not the same argument as 300 mm of bolt with a nut pulling a washer face tight. Get the post size and wall before choosing the route, not after.
Between a drive-in gudgeon on a tube post and a through-bolted one, the through-bolt is the answer for any gate opened by hand several times a day. It costs slightly more labour on site, and it is the one configuration that survives being adjusted.
Where the Clearance Actually Comes From
Every swing puts a turning effort into the same few square millimetres of plate and the hole that holds the bolt. The page names washers and nuts as the fitting for the through route because the washer face spreads that effort across the plate instead of concentrating it on the rim of the hole.
Skip the washer, or run a backed-off nut, and the hole elongates. An elongated hole is the drop. The leaf tilts, the bottom edge finds the ground or the slab joint, and the latch no longer lines up with its keeper — a hardware failure dressed up as a gate problem.
Bracing at the opening is a separate question, and this site’s guide to diagonal bracing props already answers whether a gate opening needs an extra prop. The point here is narrower: a braced post that has worked loose at its gudgeon is not braced any more.
The Latch and the Drop Bolt Do Different Jobs
Two parts keep a gate behaving, and they are not substitutes. The latch is a retaining device: it stops the leaf swinging open. A drop bolt is a locating device: it passes down through the bottom of the leaf into a socket or the ground so the leaf cannot move sideways out of line with the frame.
Put a latch on a double gate with no bottom location and the leaves still scissor in the wind, the meeting stile rattles, and the latch wears against its keeper. Put a bolt on a single leaf that needs holding shut and you have a gate that stays aligned but opens on the breeze. Both complaints reach the supplier as “the hardware is faulty”.
Here is the honest gap. The thread-length table read for this article is a hinge table; the product title covers hinge and latch, and the hardware shown in the media library runs to bolts, chain hooks and clamps. Nothing published states a drop bolt specification for a site gate — engagement depth, spring action or socket type — so that is a confirmation to request part by part, not a figure to assume. Ask three things per opening: which part retains the leaf, which part locates it, and what the locating part lands in.
Six Lines That Settle a Gate Order
A gate order fails when hardware rides along as a footnote to a panel count. Six lines, each answered in writing, closes it.
| Line on the order | What must be answered |
|---|---|
| Gudgeon route | Through, screw-in or drive-in, named gate by gate |
| Stud and thread length | The ø20 × 70 mm stud with 300 / 350 mm or 150 / 200 mm bands, matched to your post in writing |
| Post size and wall | Not published for site gate posts — get it in writing |
| Retaining and locating part | Latch per leaf; bolt where alignment is needed, and what it lands in |
| Finish | Hot dip galvanised or dacromet, stated rather than left to the range |
| Spares | Extra nut and washer sets, one spare hinge per gate, as a count |
The commercial frame matters as much as the columns. The panel minimum is 100 panels, bulk production runs 20 to 25 days, stock lines dispatch in 7 days and a quote comes back inside 24 hours. Whether hardware counts toward that minimum, or ships as its own line, is not published — so ask it in the same email as the panel count. Ten welded lines at up to 2,000 sets a week covers panels at volume, but loose bolts added to an order already cut is a picking problem: put hardware on the original order and it travels with the panels.
Frequently Asked Questions
What is a drop bolt on a temporary fence gate?
A pin or bolt that drops through the bottom rail of the leaf to hold it in line rather than hold it shut. On a double gate it stops the leaves scissoring. No engagement depth for a site gate version is published here, so confirm it per opening.
Which hinge fixing holds a site gate best?
The through gudgeon, on the numbers published. Its 300 mm or 350 mm thread clamps the plate with a nut on the far side, so holding force does not depend on what the post tube gives you. Confirm the post section before choosing the shorter routes.
Does AS 4687 tell you what gate hardware to fit?
Only if your authority says so. AS 4687 is cited on this site for temporary fencing panels, and nothing read for this article publishes a gate-hardware figure under it. Obligations vary by state and land manager, so put the bolt spec to your supplier and to whoever signs the perimeter plan.
A gate has already dropped. What is the first move?
Check the fixing before blaming the leaf. Pull the nut, inspect the hole in the plate and the washer face, and replace the fastener set rather than re-tightening an elongated hole. Where the post allows it, converting to the through route is the durable answer.
Conclusion
A sagging gate is a fixing asked to do more than its thread length and its hole can hold. The published hinge table gives real columns to work with — three gudgeon routes, one stud, two thread bands, washers and nuts — and stops there. It cannot tell you the post you are fixing into or the duty your opening demands, and those two answers decide whether a gate gets adjusted or replaced.
Lay that table beside your gate list before the next order: opening by opening, gudgeon route, retaining part, locating part, finish.